65% POLIESTER/POLYESTER
35% BAWEŁNA/COTTON
WYTRZYMAŁA NA ROZDZIERANIE I TARCIE
NISKA KURCZLIWOŚĆ
TRWAŁE KOLORY
ODPORNA NA ZAGNIECENIA
WYSOKI KOMFORT UŻYTKOWANIA
SPEŁNIA WYMOGI LEASINGU ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 60ºC
TKANINA BRIGSTON NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
PN-EN ISO 20471:2013 (*HV KOLORY)
250 g/m² 150 cm TWILL
.
65% POLIESTER/POLYESTER
35% BAWEŁNA/COTTON
WYTRZYMAŁA NA ROZDZIERANIE I TARCIE
NISKA KURCZLIWOŚĆ
TRWAŁE KOLORY
ODPORNA NA ZAGNIECENIA
WYSOKI KOMFORT UŻYTKOWANIA
SPEŁNIA WYMOGI LEASINGU ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 60ºC
TKANINA PREMIUM 240 NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
240 g/m² 150 cm TWILL
64% POLIESTER
33% BAWEŁNA
3% ELASTAN
MIĘKKA I ELASTYCZNA
WYSOKI KOMFORT UŻYTKOWANIA DZIĘKI DODATKOWI ELASTANU
WYTRZYMAŁA NA ZAGNIECENIA, ROZDZIERANIE I TARCIE
STABILNOŚĆ WYMIARÓW
TRWAŁE KOLORY
TKANINA OLIMPIA ELASTIC NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
165 g/m² 150 cm TWILL
.
.
65% POLIESTER/POLYESTER
35% BAWEŁNA/COTTON
WYTRZYMAŁA NA ROZDZIERANIE I TARCIE
NISKA KURCZLIWOŚĆ
TRWAŁE KOLORY
ŁATWA W KONSERWACJI
WYSOKI KOMFORT UŻYTKOWANIA
ODPORNA NA ZAGNIECENIA
SPEŁNIA WYMOGI LEASINGU ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 60ºC
TKANINA METEOR NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
285 g/m² 150cm TWILL
.
65% POLIESTER/POLYESTER
35% BAWEŁNA/COTTON
WYTRZYMAŁA NA ROZDZIERANIE I TARCIE
NISKA KURCZLIWOŚĆ
TRWAŁE KOLORY
ŁATWA W KONSERWACJI
ODPORNA NA ZAGNIECENIA
MEDICO KOLOR SPEŁNIA WYMOGI LEASINGU ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 60ºC
MEDICO WHITE SPEŁNIA WYMOGI LEASINGU ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 95ºC
TKANINA MEDICO NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
CEN/TS 14237:2015-12
195 g/m² 150 cm TWILL
..
65% POLIESTER/POLYESTER
35% BAWEŁNA/COTTON
WYTRZYMAŁA NA ROZDZIERANIE I TARCIE
NISKA KURCZLIWOŚĆ
TRWAŁE KOLORY
ŁATWA W KONSERWACJI
WYSOKI KOMFORT UŻYTKOWANIA
ODPORNA NA ZAGNIECENIA
OLIMPIA KOLOR SPEŁNIA WYMOGI LEASINGU ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 60ºC
OLIMPIA WHITE SPEŁNIA WYMOGI LEASINGU ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 95ºC
TKANINA OLIMPIA NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
CEN/TS 14237:2015-12
165 g/m² 150 cm TWILL
.
.
65% POLIESTER/POLYESTER
35% BAWEŁNA/COTTON
WYTRZYMAŁA NA ROZDZIERANIE I TARCIE
NISKA KURCZLIWOŚĆ
TRWAŁE KOLORY
ODPORNA NA ZAGNIECENIA
WYSOKI KOMFORT UŻYTKOWANIA
SPEŁNIA WYMOGI LEASINGU ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 60ºC
TKANINA CANVAS NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
260 g/m² 150 cm CANVAS
.
.
65% POLIESTER/POLYESTER
35% BAWEŁNA/COTTON
WYTRZYMAŁA NA ROZDZIERANIE I TARCIE
NISKA KURCZLIWOŚĆ
TRWAŁE KOLORY
WYSOKI KOMFORT UŻYTKOWANIA
SPEŁNIA WYMOGI LEASINGU ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 60ºC
TKANINA MORO US NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
250 g/m² 150 cm TWILL
. .
65% POLIESTER/POLYESTER
35% BAWEŁNA/COTTON
PODWYŻSZONA WYTRZYMAŁOŚĆ NA ROZDARCIE I PRZETARCIA
NISKA KURCZLIWOŚĆ
TRWAŁE KOLORY
DOBRA PRZEPUSZCZALNOŚĆ POWIETRZA
WYSOKI KOMFORT UŻYTKOWANIA
TKANINA SPEŁNIA WYMOGI LEASINGU ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 60ºC
TKANINA RIBBON NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
245 g/m² 150 cm RIP-STOP
60% BAWEŁNA/COTTON
40% POLIESTER/POLYESTER
WYTRZYMAŁA NA ROZDZIERANIE I TARCIE
NISKA KURCZLIWOŚĆ
TRWAŁE KOLORY
KOMFORT UŻYTKOWANIA
ODPORNA NA ZAGNIECENIA
SPEŁNIA WYMOGI LEASINGU, ZE WZGLĘDU NA WYTRZYMAŁOŚĆ MECHANICZNĄ PO 50 CYKLACH PRANIA I SUSZENIA BĘBNOWEGO W TEMPERATURZE 60ºC
TKANINA JUPITER NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
315 g/m² 150 cm TWILL
100% POLIESTER/POLYESTER
WYKOŃCZONA PU/WR
WYTRZYMAŁA NA ZAGNIECENIA, ROZDZIERANIE I TARCIE
STABILNOŚĆ WYMIARÓW
TRWAŁE KOLORY
BOGATA KOLORYSTYKA
WYSOKI KOMFORT UŻYTKOWANIA
ODPORNA NA WILGOĆ
DOSKONAŁA POD NADRUK
TKANINA OXFORD PU/WR 200 NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
PN-EN 71-2 + A1:2014
PN-EN 71-3 + A1:2014-12
PN-EN 1888
PN-EN ISO 20471:2013 (*HV KOLORY)
200 g/m² 160 cm PLAIN
100% POLIESTER/POLYESTER
WYKOŃCZONA PVC
WYTRZYMAŁA NA ROZDZIERANIE I TARCIE
NISKA KURCZLIWOŚĆ
TRWAŁE KOLORY
BOGATA KOLORYSTYKA
WYSOKI KOMFORT UŻYTKOWANIA
ODPORNOŚĆ NA WILGOĆ
DOSKONAŁA POD NADRUK
TKANINA KODURA 350 PVC NORMY
PN-P-84525:1998
PN-EN ISO 13688:2013-12
PN-EN 71-2 + A1:2014
PN-EN 71-3 + A1:2014-12
PN-EN 1888
350 g/m² 150 cm PLAIN